+++++++Dear Friends,
We are providing services of vibrofinishing for one of the world's leading sintered component manufacturing companies. We are doing this process for last ten years in diesel base vibrofinishing compounds to avoid rusting problem. We want to shift this process to waterbase barelling without using a dryer.
So would like to know if there are any such chemical which can prevent rusting if used in waterbase barreling.
Thank you.