have a set of motorcyle wheels that are chrome. I am want to either paint or powdercoat them. do I need to have the chrome stripped off of them or can I just spray it.

Jeremy Wilson
buyer - Whiteland, IN, USA


+++++++

Paint (or powder) won't stick to chrome. Some powder coaters report good results with a light sandblast, but it may be necessary to acquire some skill at it (have never actually done it myself).

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search