Copper Patina works on solder but won't take on lead came

+++++++

I am having a problem getting my copper patina for lead to work on my glass project. The copper for solder worked fine but even after days of applying nothing has happened on the lead. I now have a two tone panel. What is going wrong?

Carla Norrell
Hobbyist - Northport, Alabama


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search