Hardchrome plating emission limits for open electroplating tanks

+++++++

Dear Sir

What is the emission limit for open tanks during hardchrome plating?
Note that We are not using any fume suppressant in our tanks.
please help!

Best Regards

Mohsin Siddiqui
Assistant Manager - Karachi, Pakistan


+++++++

Hi Mohsin,

The U.S. specs for chromic emissions are very tough, ie. 0.05 mg/cu M....maybe too tough.

The specs back in l978 in B.C. were ll grains of sulphuric/chrome per 1,000 cfm (or was it per single
cfm, I forget).

Using an ordinary but very well built CT-120/2 blade type eliminator, we achieved 0,34 grains .... that's equivalent to 30 times lower than those specifications BUT translated into metric, it's only O.7OO mg/cu.M Yes, I have that in writing.

You definitely need some exhaust.

Does this help?

Freeman Newton - White Rock, British Columbia, Canada
Ed. note:
Please keep Freeman in your thoughts
& prayers.


Message from Freeman, Dec. 2010

Ed. note: Welcome back, Freeman, and get back to 100 percent soon.


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search