Paint is peeling off in sandwich panel fabrication despite passing all lab tests

+++++++

We have prepainted 300 mt of material and found all properties ok in our laboratory but it is failing at our customer end while making sandwitch panels at the edges where the sheets are T bended under under load.The paint is craking at the bent areas even though ot test was passing in our laboratories.Please suggest.

Yogesh vaswani
Jr.Manager - Nagpur


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search