Heavy grease removal

+++++++

We are in rebuilding of auto electrical units, and lots of old parts( heat treated carbon steel) have lots of grease in it, mostly the grease is lithium based. We generally make use of manual brushing or solvents like MC or IPA, but its very time consuming and cumbersome. Is there any way to simply dissolve the grease by just immersion or any other method, we do the shot blasting after the grease removal.

G.S.ARORA
buyer,regulator - DELHI, INDIA


+++++++

Hello Arora g
U just make a detergent based highly alkali bath & maintain a 60 - 70*c temp. then dip ur parts into for 5 - 6 minutes then follow the procedure with same solution & temp. bath with anodic current of low volts D.C.

Kuldeep Singh
Wet process engineer - Pantnagar, Uttrakhand, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search