Quick Analysis of Chrome Bath

+++++++

Is there a procedure available for checking Cr +6, Cr + 3 in chrome bath using spectrophotometer? What is the wave length at which one can detect Chrome?

Kaushik Magiawala
plating shop employee - Gandhinagar, India


+++++++

You may want to get the book "Colorimetric Analysis of Metal Finishing & Metal Working Solutions & Effluents" by Aubrey Knowles that will describe various methods. If not, you can try a simple direct method with hex chrome at 370 nm and tri chrome at 640 nm. Dissolved iron will likely interfere with the hex chrome measurement, but it may be accurate enough for your purposes.

Jon Barrows, MSF, EHSSC
Chemical Process Engineer

Polyfab Plastics & Supply

Springfield, Missouri


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search