How to convert fine brush finish into coarse brush finish on SS304 sheet?

+++++++

I have SS304 1.2mm thick sheet parts (Size 128 mm x 230mm). The sheet already has a brush finish on it when I bought it. However, the brush finish on it is very bright and fine, while my other components which ultimately have to be assembled along with this item have coarser and less bright finish compared to this.
Please suggest how I can convert this fine brush finish into more dull & coarse finish?

Thank you in anticipation.

Rishi Dass
Manufacturer - DehraDun, UA, India


+++++++

This would be done mechanically rather than chemically, Rishi. You would probably use scotch brite or sandpaper on a large flat belt sanding machine. As in everything else, skill and experience help; so you may want to contract it out.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search