Sir
We are an electrical switch gear company and we are doing silver plating on a copper part. basically it's a contactor of starter. The coating thickness of the plating is around 6-10 microns. Our customer is SST, 96 hrs.pass on this contactor
My Question: is
is SST is an appropriate test on silver palting.where as the base metal is copper?

Dinesh Chandra
Manager Paint shop - India


+++++++

I would not call it common, but it could be used. You would have to look for green corrosion rather than red or white.

James Watts
- Navarre, Florida

+++++++

With reference to the previous query I have three questions.

1 - What should be the salt spray hours for silver plating on copper part.(plating thickness is 2-3 micron.)
2 - Is the SST is a recommended test for silver plating.
3 - Is there any reference in ASTM where we can find out the coreletion between plating thickness and SST hours.



best regards

Dinesh Chandra
- India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search