44083

Seeking Cadmium - Titanium Alloy Plating per STP58-005

February 21, 2007

We need Cadmium Plating-Titanium Alloy Plating per STP58-005 Class II for the following Part Number:
4F23553-105B / Link, Lock Assembly (Qty. 2 Ea.) *** EXCEPT OMIT BORES ***

OK to OMIT steps 3.3.5-3.3.3.5.2.1 (Cyanide Bath). Work can be done IAW SPEC STP58-005.