44069
What is zinc ash and bottom dross loss?
+++++++
What is the normal ratio of the Zinc ash and bottom dross compared
with the consumed Zinc in hot dip galvanization and how I can recover
pure Zinc from the ash and dross effectively. I am a manager and
producing galvanized wire by hot dip process and the Zinc lost
through dross and ash is really bothering me much.So far I remelted
the ash (big sizes) in a curicible and recovered metallic Zinc.I have
also used ammonium chloride but not found very effective.How can I
increase the effectiveness.Is there other additives to mix with the
ash and dross?
If you could give me some recommentation it will be very appreciated.
Süleyman
BEÞLÝ
ÖZYAÞAR A.Þ - Silivri-ISTANBUL, TURKEY
+++++++
Could you please answer how I can reduce the smoke(fume) created
during hot dip galvanization on the Zinc furnace and reduce the zinc
ratio retained in the ash?
Süleyman
BEÞLÝ
--ISTANBUL, TURKEY


 |