Reduce electro-nickel plating cost
[India]
February 17, 2007
I am electro-nickel plating small components in barrels. Now with
the cost of nickel skyrocketing, I am not able to control my costs.
Kindly advice.
Thanks,
Dinesh Samuel
- Chennai, India
February 18, 2007
Atotech used to market a
nickel-iron plating process to deal with this same issue. I don't
know if it still exists, but you might inquire.
|
|

Ted Mooney, P.E.
finishing.com
Brick, NJ
|
February 20, 2007
You do not say what your end use is, so we don't know what youe
actually need. However, try looking at white bronze plating.
|
|
Trevor Crichton
R&D practical scientist - UK
|


 |
|