Salt Spray Test Hours for crca sheet panels and cabins

+++++++

Salt Spray test in hrs
for the following product achievable
Product CRCA PANELS /CRCA CABINS
PROCESS FOLLOWED
1.Pretreatment Hot Degrease + Water Rinse and Hot Zinc Phosphate + water Rinse (Spraying Process)
followed by water drying oven
2. Primer coat
3 primer coat Baking
4 Top coat
5 Top coat Baking

What we want to know the number of salt spray hours achievable for this product.

Vijay D Phadke
Trutek Systems Combine Privt Ltd - Pune, Maharashtra, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search