Coating Al2O3 on a 150um Pt sphere

+++++++

In my research I need to coat a Pt sphere with ~150um diameter with a layer of Al2O3. The thickness of the coating is not critical, as long as it can cover the Pt sphere. However, previous experience shows the thickness cannot be more than 2um, otherwise it is easy to be broken. Sputtering can do this kind of coating. The problem is how to hold this tiny sphere. Some people use tape to hold this sphere. After one side is coated, manually turn the sphere to other side and coat it. It is greatly appreciated if any other ideas are given on this problem.

Xueyang Yu
University of Western Ontario - London, Ontario, Canada


+++++++

Maybe figue a way to roll it instead of keeping it from rolling.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search