43082
Need electrodeposition of lacquer for
silver
++++++
I WANT START A PLATING SHOP FOR JOB WORK.I WANT TO AVOID SPRAY
LACQUER BECAUSE THE COLOR OF SILVER GETS DULL.Please let me know the
address of manufacturer & material suppliers.
RAKESH JAWA
ELECTROPLATING - MORADABAD, U.P., INDIA
++++++
The best would be to get in touch with the electrophoretic
chemical suppliers. They will in turn guide you on from whom to
source the equipment. Almost all electroplating chemical suppliers
also supply electrophoretic lacquer - Progressive, GW, Artek,
Atotech are a few which come
to the mind off hand.


 |