43075
Addition of Cadmium metal in Cadmium
Plating Bath
++++++
We analyse Cadmium Plating Bath for cadmium metal, Chlorides and
Sulfates. Cadmium metal content of the bath is at lower limits. We
have Cadmium anodes dipped in the bath but it increases metal content
very slowly. How can we add Cadmium metal other than anodes to the
bath already prepared.
thanks.
Zakir Shah
chemical engineer - Karachi, Pakistan
First of two simultaneous responses -- ++++++
You use cadmium oxide. Wear a respiratory mask so that you do not
inhale any as it will give a dust cloud if you are not extremely
careful.
James Watts
- Navarre, Florida
Second of two simultaneous responses -- ++++++
Simply put cadmium oxide into a filter bag and hang into plating
bath with circulation can increase cadmium content.

David Shiu
- Singapore
++++++
You generally add cadmium oxide. I suggest you get a reference
book.
Gene Packman
- Great Neck, NY


 |