Is it ok for copper pipe to touch a brick or a rock in the backyard. I recently had a copper repiping done and they had to bury the pipes to connect the house to the garage but I noticed that they did not support the underside of the pipes with a rock or a brick. I wanted to make sure this is ok since galvanized metal touching a mortar is suppose to introduce corrosion. Thank you.

Takashi Fujii
DIY - Long Beach, CA, USA


++++++

Galvanized (zinc) materials as well as aluminum can be sensitive to the alkaline content (lime) of concrete. But copper and bricks sound perfectly compatible to me.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


++++++

Thank you very much! I will move forward on that project.

Takashi Fujii
- Long Beach, CA, U.S.A.





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com