Why does my titanium anodizing dull when touched?

 

++++++

Why my titanium colour by anodizing will turn down brightness when use my finger touch it?

I had put it in boil water one hour.Why? Please help me?Thank you !

Steven Li
- China


March 27, 2008

Dear Mr. Li
As you know colors appeared on anodized titanium surfaces are exactly depended on thickness of oxide layer which is a transparent layer. these colors are known as interference colors,so when the surface is coverd with any contamination the colors will be changed (for example brightness will be changed or ...).
when you touch a surface of anodized titanum, a thin layer of oil will be remaind on this surface. if you wash the contaminated surface with any detergent, the orginal color will be appeared again.

Shahram Ghahremani
- Tehran, Iran


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search