We are renovating our bathroom and I have seen an advert for a
stainless steel heated towel rail. It says they are better quality
than chrome, and will not rust or mark like chrome. Is this true? Do
they have the same durability? I have looked everywhere for some
product information on this, but no one can tell me the
advantages/disadvantages of both.
Hope this isn't a silly question to you.
Kind regards
Liz
Elisabeth Biec
home renovation - Auckland, New Zealand
November 16, 2006
It's not the least bit silly, but opinions will vary. The chrome
plating will look better but probably not last as long. Truly high
quality chrome is a great finish (witness truck bumpers) but lower
quality chrome plating can be a very poor finish and it's hard to
know which you'll get.

Ted Mooney, P.E.
finishing.com Inc. - Brick,
NJ


 |
|