Auxillary Anodes in Cu and Ni  

++++++

Our metal levels in our Ni baths and Acid Cu baths rises and they need cut pretty regularly , on average about once every 4 months. I know that we should be able to reduce our anode area to lower the amount of metal build up but its just not a practical solution our problem.

I was wondering if its possible to use Titanium or Graphite anodes as auxialliries but hang them next to our normal anode baskets to help lower the metal content of the solution.