Letter 42095

Size buildup of manganese phosphate plating on G2 CAST IRON  

++++++

Hello,
My name is Buzz,I work for a precision machining co. in PA.WE have a new job we need some help with. We're machining G2 Cast Iron (hardened & tempered to 250-300 BHN).It is cylindrical in shape (8.5" long x 2.5" O.D. x 1.7500"-1.7510" dia. bore after plating). How much size buildup should we allow for from the manganese phosphate plating to hold the close tolerance bore?
Any help would be greatly appreciated.
Thanks,

Buzz Ponitz
Precision machining - New Stanton, PA, U.S.A.


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com