Need stain line conveyor coating
++++++
I AM LOOKING FOR A PRODUCT THAT I CAN COAT MY STAIN LINE CONVEYOR CHAIN WITH. THE STAIN IS A WATER BASE STAIN AND AFTER ABOUT TWO MONTHS IT STARTS TO BUILD UP ON THE CONVEYOR CHAIN AND ATTACHED PARTS. A SPRAY ON SUBSTANCE WOULD BE THE EASIEST. TEAR DOWN AND CLEAN UP OF MY STAIN LINE IS EXTREMELY LABOR INTENSIVE.
TIM MALLMANNMANUFACTURER - CHILTON, Wisconsin
----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!