Would nickel tubing work for the stem drilling process (elcetrochemical machining) in place of titanium and ss tubing for deep hole drilling in alloy materials.

Andrew Cousins
ac - Houston, TX, USA


December 4, 2007

To answer your question, no. teflon coated Titanium is the only material to be used for STEM. I have done STEM work for over seven years until recently.