Argentium [Bolivia] 

June 7, 2006

When I cast argentium after polishing a piece, black stains appears on the surface. I can not remove it pickling or polishing.

Where is the problem?

Adriana Cuellar
AJM - Santa Cruz, Bolivia


September 12, 2006

This looks like fire scale. Most likely your flask was too hot or your melt was too hot or both.

Neil Bell
Red Sky Plating - Albuquerque, NM, USA


First of two simultaneous responses -- December 1, 2006

That is fire scale, it can be removed with agressive polishing.

Marc Banks
Blacksmith - Elizabeth City, NC, USA


Second of two simultaneous responses -- December 3, 2006

You can use a chemical solution for cleaning and Ag surface pasivation(to be maintain clean a long period!).

ALEXANDRU SAVU
SC SAVPROD SRL - Bucharest, ROMANIA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com