Mirror finish on stainless steel surface  

++++++

i am a stainless steel cutlery manufacturer. i need to know how to bring about mirror finish polishing on stainless steel. please let me know the ingredients to be used and the method by which to do the same. also how to do mat finishing too.

Harish Shah
H K Kitchenware - Mumbai, India


++++++

This is a very very broad question, Harish. So please start by describing what mechanical or chemical finishing you presently employ, and what finish it gives you that is neither shiny not matte. Thanks.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


++++++

Dear Sir
I suggest electropolishing for your cutleries that is what we are doing.

with regards,

Kandaswamyraveendhran
metal finishing - Coimbatore


++++++

You can make electrochemical polishing by max. sulfuric and phosphoric acids 40 : 60

Ali Gomaa
- Cairo, Egypt


++++++

Use chromium oxide for final polish(or very fine corundum dust). Second option is electropolishing. Good luck!

Goran Budija
- Zagreb, Croatia


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com