Letter 42036

What cause electroplating bleed out at casting coner edge and how to overcome?  

++++++

I am working as a production manager at a pressure Aluminum die casting house and our casting product mainly for hard disc industrial.
Our raw casting required eletroplating process and we face e-coat bleed out defect.
Can someone please provide a solution.

LEE LEONG HUA
Aluminum pressure die casting - Malaysia


++++++

Mr Lee

The problem is complex . It requires Hands on solving at site.

Reasons for bleed out are many.

Unless we know what you are doing and How, it will be quite difficult to come back with a meaningful solution which, I suggest is best handled by a professional, at SITE.

Regards,

Asif Nurie
Atlanta Global Limited

New Delhi, India


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com