Letter 42033

Chromium Mirror Coating Parameters  

++++++

We are exploring the production of Automative Mirror coating by Chromium Sputtering
onto glass. We are getting coating of good reflectivity but it can be easily scratched.
What may be causes for this?

What are the typical process parameters? What should be the DC voltage and chamber pressure? Also, what is the requirement for substrate glass cleaning? Should it
be only cleaned with deminineralized water or by organic solvents? Is ultrasound
cleaning necessary?

Thanks,

Dr. Sunil V. Gokhale

Sunil Gokhale
Advanced Process Technology Pvt. Ltd. - Pune, India


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com