Gravimetric test for determination Al and Pb % in Zinc Bath  

++++++

Dear All:
can you please provide me with a chemical test (gravimetric) for determination of Al and Pb in zinc metal.

Salah Salman
- Cairo, Egypt


++++++

Sir,
Check out my articles in the magazine Metal Finishing.
(1)"Test for Lead in Hot-Dip Galvanizing Zinc" Metal Finishing pages 29-31 October 1991.
(2)"Aluminum Control in Galvanizing Kettle Zinc" Metal Finishing pages 61-63 March 1983.
Copies of both articles can be obtained from a large library though interlibrary loan for xerox charges.
A spectrophotometer (flame) in absorption mode using air as oxidizing agent is best for lead and in the emission mode using nitrous oxide is best for aluminum. A one gram sample of kettle zinc is dissolved in 40 mL of dilute nitric acid and compared with standards on both sides of the sample. ICP (Inductively coupled plasma) likely would work but I have no experience with ICP.
Regards,

Dr. Thomas H. Cook, Galvanizing Consultant

Hot Springs, South Dakota, USA


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com