Sir,

Please tell me the detail latest process for Powder Coating Pretreatment Process for M.S. sheet.(thickness 0.5 to 1.5 mm). And please tell me the frequently appeared causes for rejection (Troubleshooting) and remedies.

thanking you,

HRISHIKESH TA
LIGHTING - MUMBAI, MAHARASTRA, INDIA


++++++

Hi, Hrishikesh. You need to retain a consultant for this pretreatment, or align yourself with a proprietary supplier who will help you, or at least get hold of a book or two on pretreatment such as Samuel Spring's "Preparation of Metal for Painting" [link is to info about the book at Amazon] or "Phosphating of Metals" [link is to info about the book at Amazon] by Werner Rauch.

There are numerous approaches to pretreatment ranging from iron phosphate to zinc phosphate to proprietary modified phosphates to zinc plating to electropriming, and each of these has numerous variations. Unfortunately there is no way to say which is most appropriate for your situation without a detailed study. Good luck.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search