Ballizing process  

++++++

I do a hand ballizing operation with an Arbor press in some bushings. Right now we have to use multiple balls to expand the hole and obtain the desired finish for a .2187 ball to ride smoothly in it. How much clearance should I need to be able to ballize this hole just once. Does it depend on the material and bore finish?

Dan Parsons
- Athol, Massachusetts


++++++

Clearance? Maybe you referr to interference (ball being greater than bushing). It depends on the elastic and plastic (temporary and permanent deformation) properties of the particular part, which in turn, depend on the material, hardness and shape. The issue here is the friction between ball and bushing making it more difficult to obtain the desired results w/o galling, seizing, etc.

Guillermo Marrufo
Monterrey, NL, Mexico


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com