Hi,
We are a distributor. We are looking to replace some stainless parts
w/ alloy parts w/ a bright finish as similar as S/S. People have
mentioned maybe nickel or Chrome. My problem is that it has to be
ROHS compliant. What do you suggest?
Steve Smith
Distributor - Elk Grove, IL USA
June 9, 2006
Both nickel plating and chrome plating are RoHS compliant, Steve.