I would like to know if Zinc Plated items such as Grilling and Roasting Racks are safe for use on BBQ's
If Not, apart from Stainless Steel what would be the best plating to use for such BBQ racks and Utensils

Regards,

Allan Butler
trading - Brunswick, Victoria, Australia


++++++

I'd say they should be nickel plated. Not so much as a matter of safety but as a matter of durability. BBQs are hot enough to vaporize the zinc. Alternately, ceramic coated.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


February 16, 2010

I suggest to plate with electroless nickel

alfonso meza
- san jose California

EEH book
Electroplating Engineering Handbook

Lawrence Durney


Mallory book
Electroless Plating - Fundamentals & Applications,

Mallory & Hajdu


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search