Deposit of coating on screw threads

Dip-spin Coating Services pointer 

++++++

We are doing Dacro Coating by Dip Spin process. We are facing problem with coating deposit on screw threads which results in gauge not qualifying.

Sanjay Chitlangia
aum dacro - Gurgaon, India


++++++

You really should be talking to the Mfg's tech services. It depends on what you call a screw also. You can not expect to coat a 10 x 40 one and have it pass. A half inch bolt is another story.
Basically, if it is possible, it sounds like a thinner material that you are dipping in and a faster or longer spin, possible sooner.

James Watts
- Navarre, Florida

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search