I have a piston type machine for manufacturing compressed sawdust firleogs. This machine is really very basic and has only four wear parts. Namely a piston head, wear nut, taper and wear sleeve. The finished product firelogs are 75mm diameter.

The taper and wear sleeve need to be frictionless to manufacture a good log and highly abrasive resistant to last. Can somebody please help me to find a suitable abrasive resistant and low friction coating or steel / treatment for these wear parts.

Gerald van den Blink
firelogs - Cape Town, South Africa


++++++

There are certainly alternatives, and some may even be better, but the 'standard' time-proven approach for components like this is hardening the steel and then hard chrome plating it. Good luck.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com