Letter 41003

Powdercoat peeling [New Jersey] 

June 5, 2006

I had an automatic pool cover installed last fall and the coating is peeling off the aluminum track and box cover as though it was painted....the finish looks different from the powdercoating finish on my patio furniture and I don't understand why.

Judith A. Jacoby
Homeowner - Middletown, NJ, USA


November 29, 2006

Dear sir,
First thing powder coating peeloff has folowing main reason:-
1.Poor pretreatment(Chromatizing prefered for Aluminium object), it is not properly degreased.
2.Poor powder coating baking that means under baking.
3.Their may be powder problem.
Second thing when powder is peeling thats why it is finish not look like o.k.
Thanks
With regards,

Sanjay kumar Jain
- INDIA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com