HARD ANODISING COLOUR
-
Dear sir,
We are facing the following problems in our Hard coat Anodising. Patchy marks like small round, found after hard anodising. In these areas colour is dull, and we tried with regular cleaning methods only. please advise us how to avoid this, can we do any special pre cleaning process or this is a raw material problem.
ELANGOVAN
- INDIA
Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.
If you are seeking a product or service related to metal finishing, please check these Directories: