Electroplating onto Aluminum with Copper Sulphate, Nitrate, or Chloride

-

I am doing a project on electroplating and I'm going to use Copper Sulfate, Copper Nitrate, and Copper Chloride. I'm going to see which is more efficient in plating aluminum. I have ordered 100 g of each. I will have to do 10 trials of each. I was wondering what would be a constant voltage I could use and how do I calculate the amount of water to mix with each to get a 1 mol solution. Also how long should each trial last.

Trey McCants  
- Seneca, South Carolina


-

Uh, Trey, uh who designed this experiment?  :-)

I don't know why you intend to use aluminum, but . . .

You cannot plate onto aluminum without special techniques and chemicals you don't have access to. Further, you cannot electroplate a more noble metal (copper) onto a metal which is less noble (zinc, aluminum, or steel) without totally screwing up your experiment because it will spontaneously plate out without external electricity. Ideally you should use real silver dimes or quarters as your substrate, although nickels or modern dimes or nickels will suffice.

A 1-1/2 volt D-cell battery will do fine. You ideally should put a resistor in series to limit the current to no more than about 5 amps per square foot, and use a pocket milliammeter to measure and verify the current.

I'm sure you know what a molar solution is and are really asking the formula weight of these three salts. Well, copper sulphate is CuSO4.5H2O; copper chloride is CuCl2.2H2O; I don't know how hydrated copper nitrate is, but the formula will come with the material.

The electroplating should probably go on for about 15 minutes, and Faraday's Law ("96,500 amp-seconds will deposit 1 gram equivalent weight") will predict the thickness of the copper layer for you. Good luck.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+

Dear Sir:

I was planning to have a copper plating on an iron steel. I tried using sulfuric acid and copper chloride solution but the output is a black coating. What should I use to have a clear copper plating and what is the typical current and voltage in plating with copper.

David CabaÒal
- Iloilo City, Philippines

+

Cyanide copper plate at 10-30 amperes/square foot, 1-5 volts.

tom portrait
Tom Pullizzi
Falls Township, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search