Electropolishing for Nitinol wires

-

My name is Emanoel R. of Almeida, and I work in a parts factory for use orthodontics. I seek information on equipment and composition of the electrolyte for polishing of Nitinol (Ni-Ti alloys). Some attempts, in laboratory equipment, presented embrittlement, probably due to nascent hydrogen. Any information is of a lot of help. Thank you advance / Best Regards.

Emanoel Ribeiro de Almeida  
SP - Brazil


++

Nitinol is subjected to hydrogen embrittlement. Bake after your process for 30 minutes @ 400 F. You will be ok again.

Todd Huehn
- Blaine, Minnesota


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search