Preparation of stainless steel prior to plastering

-

I need to plaster over a stainless steel plate. Dimensions 50 mm x 1.3 m. I would be grateful for anybody's advice as to the correct preparation of the steel Thank you & Regards. Neil Franks

Mr Neil franks
- London, England


-

Hello Mr. Neil Franks,

The plaster will not stick directly to the steel (except by encapsulation). To deal with temp changes and high relative humidity, you will need to apply sheet rock (and maybe a moisture barrier) or metal lath to the steel for the plaster to mechanically adhere.

Regards,

Fred Mueller, CEF
- Royersford, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search