Seeking Lab to do Kesternich Testing

-

I'm looking for a source for Kesternich testing per DIN 50018 [link is to spec at TechStreet]. Does anybody have a reliable lab they can refer me to?

Christa Shirey
- Sylvania, Ohio


-

Hey Christa,

Kesternich: German scientist who developed the Kesternich Cabinet and test method used for acid rain simulation (DIN 50018).

U.S. INTEC, Inc. tests their Roofing and Building Fasteners using the Kesternich test. Talk to the tech people at U.S. INTEC, Inc. Port Arthur, Texas.

Hope this helps,

Fred Mueller, CEF
- Royersford, Pennsylvania


+

Christa Shirley, for Kesternich testing contact SGS U.S.Testing Co., Fairfield, NJ

John D. Dooley
fasteners - Long Beach, California


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search