hi!!! I'm a student from the Philippines and I'm greatly in need of your help. i have this job to do to report about the whole process of gold plating but there's are major problem... i don't know the complete process of gold plating and any idea of it whatsoever... and i need to know it very soon - or I'll be dead meat... do u think u could help me with my problem??? thanks anyway for taking the time to read my letter and good luck!!!

MJ BP
- Philippines


March 1, 2009

Hi, MJ. You should see if your school or town library can find some books on this for you:

Gold Plating Technology by Reid & Goldie would be a great one. But you should be able to find a good introductory chapter in most plating texts like the Metal Finishing Guidebook or the Electroplating Engineering Handbook.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com