Method for Touching Up Powder Coating 

-

Our customers require us to assemble Powder Coated parts. Sometimes they are pitted or damaged. Is there a way to touch-up Powder Coating or Handling defects?

A. Korselman
- San Francisco, California


-

Dear Mr A Korlselman,

This query has been answered by me on an earlier letter but at the risk of repeating myself here goes:

Dissolve the same powder used in the coating in TC or any NC based thinner in which the powder dissolves. Touch up the scratched area with the resultant Paint /paste/ liquid powder whatever you call it with a suitable paint brush.

Experience will give you an idea of how much your Solvent/ powder mix should be.

All the best,

regards, K Vahanwala

Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com