Graphite cathodes for anodizing of aluminum?

-

I have a customer who does type II anodizing. he is requesting graphite cathodes. However, I have no idea what type of graphite to use, or sizes of cathodes. tank is 6' x 3' x 42" deep (36" solution level).

Can anyone give me pointers?

Thanks in advance

Bruce

Bruce OBrien 
- Chandler, Arizona


March 1, 2009

Hi, Bruce. Letter 1177 talks a bit about graphite anodes and says they are part of the Sanford process.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search