SharkSkin to protect Aluminum from Water Staining 

-

Does anyone know of a wipe-on product called SharkSkin that is claimed to protect aluminum from discoloration due to oxidation and water staining?

Gary Nitowski
- Alcoa Center, Pennsylvania


.

Have not heard of SharkSkin, however Everbrite Protective Coating may be what you are looking for. It is an easy to apply, one part, self leveling clear coat which can be wiped on or sprayed on. It will refinish faded metal and protect it from oxidation, corrosion, moisture, salt air, acid rain and other damaging elements. Please feel free to contact Everbrite, Inc., Reno, NV if you have questions. Thank you, Teresa Sedmak

Teresa Sedmak
Everbrite, Inc. - Reno, NV, USA


March 1, 2009

Hi, Gary. I'd be pretty sure that a little typo slipped in and you are actually looking for "Sharkhide". Sharkhide is a product of the site's supporting advertiser, Flatwater Inc., and is described with the terms you used.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com