Gold plating peel off

++++++

We do electrolytic gold over copper (no intermediate layer like Ni) up to 3 microns.in our case it is not completely peeling off when we are cutting the parts from the panel it is occurring from the cutting edges to some extent.

JHONSON.BODDU
microwave products - HYDERABAD, AP, INDIA


++++++

Sounds like you have poor adhesion rather than no adhesion Jhonson.. Don't talk yourself into it being acceptable though :-)

It's very difficult to say what's wrong even if you gave us complete details, and so far you've given us none. Perhaps the first step is to develop a clear, quantifiable adhesion test for this particular component so that you can measure whether you are making progress.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search