Letter 40062

1045 Steel has become magnetic  

++++++

I have some carbon steel grade 1045 that is acting as a "Magnet" This is unusual.
What causes this to happen?

Tom Klueneau
- Claremore, OK


++++++

Magnetization will occur due to proximity to any magnetic source such as an electric bobbin or a permanent magnet such as a magnetic grinding table, also due mechanical work.

Guillermo Marrufo
Monterrey, NL, Mexico