Salt spray resistance for E D  

++++++

Hello every one,

what is the salt spray resistance for electro deposition coating?whether salt spray resistance is dependent on the dry film thickness?


thank you,

B SATHYA NARAYANAN
COLORSINDIA - CHENNAI, TAMILNADU, INDIA


++++++

The actual salt spray test results depend upon the substrate, the quality of phosphating and Electrocoating.

The salt spray specifications given by paint suppliers in India for Cathodic Epoxy Electrocoat on standard test panels when tested in compliance with the test standard ASTM B-117 [link is to spec at TechStreet] is 1000 hours.

Hope this answers you question.

Gurvin Singh
Coatec India -

Mohali, Punjab, India


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com