Removing unwanted splashed tin coating from outside of antique copper tea kettle

++++++

Recently purchase a nice antique dove tailed copper tea kettle. However, it has a big ugly appearance problem. Sometime long ago it appears someone did a very sloppy retining of it's interior. Question: How do I get the messy tin off exterior copper's surface? Thanks for any help!

Gloria Bowman
- Overland Park, Kansas


++++++

Try mixture of 1 part water/1 part muriatic acid [linked by editor to product info at Amazon] (conc.), 65 C temp.

Good luck!

Goran Budija
- Zagreb, Croatia


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search