Dear Sir,
I would like to know whether an organic phosphated metal sheet can be subsequently passed through Cathodic Electrodeposition process or not.If we can apply E coat on organic phosphated sheet then what are the properties of that coating - like Salt spray test ,adhesion.I would also like to know whether there is any supplier in India for organic phosphating chemicals. Thanks

RAJESH KUMAR VERMA
Assistant Manager Process Engg. in an Indian automobile co. - Pune , India


++++++


Mr Verma

In case you wish to run Ed coat over steel here is a suggestion thats environmentally friendly and will improve SST life considerably.

Plate with alkaline Cyanide-Free zinc
Yellow Chromate
ED Coat

this is being done at a few places in India and is entirely cost effective and more reliable than Phosphating.

Yes, a supplier does exist in India.

Regards

Asif Nurie
Atlanta Global

New Delhi, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search