Can anybody let me know what is the significant difference betwee these two notes listed below for Rohs compliance.
1. Underplate with 5 micron minimum Nickel. Plate with 10-15 micron matte tin to BS-6137 [link is to spec at TechStreet]
2. Matte Tin plate per ASTM
B545 [link is to spec at TechStreet], class "A" over Sulfamate Nickel per AMS-QQ-N-290 [link is to spec at TechStreet], 0.0001inches, minimum.
Thank You.
control aolutions - Bangalore, Karnataka, INDIA
++++++
The second^firstspec sounds twice as thick, Chandrashekar. But one cannot really plate in accord with a spec that one does not have. Acquiring them is probably step 1, and see if they clarify the issue. Good luck.
|